Product Code |
Metal content % |
Use |
Packing |
| I accelerating agent |
8(Co)±0.2 |
manufacture of glass fiber reinforced plastics; curing of unsaturated polyester |
25kg/plastic drum, 18kg/iron drum |
| III accelerating agent |
12(Co)±0.2 |
manufacture of glass fiber reinforced plastics; curing of unsaturated polyester resin |
25kg/plastic drum, 18kg/iron drum |
| XY-1 |
2±0.1 |
unsaturated polyester craft resin curing |
25kg/plastic drum, 18kg/iron drum |
| Y-4 |
9±0.2 |
unsaturated polyester resin pre-acceleration, curing |
25kg/plastic drum, 18kg/iron drum |
| Y-5 |
9±0.2 |
special unsaturated polyester resin pre-acceleration, curing |
25kg/plastic drum, 18kg/iron drum |
| Y-8 |
8±0.2 |
unsaturated polyester curing |
25kg/plastic drum, 18kg/iron drum |
| XY-T8A |
6±0.2 |
unsaturated polyester resin button curing |
25kg/plastic drum, 18kg/iron drum |
| XY-T8B |
6±0.2 |
unsaturated polyester(general type) curing |
25kg/plastic drum, 18kg/iron drum |
Remark: Gel time and heating peak temp. can be tailored upon clients' specific needs.